ii

i82much

08/02/2008 7:24 AM

Fuming Purpleheart

I am working on a project that is African Mahogany framed with
Purpleheart.I was concerned if I needed to treat the edge that I'm
going to glue, because of the oils (like Teak). It was suggested that
I fume the purpleheart with muratic acid.
I had seen the fuming process done with ammonia, but never with acid.
Has anyone ever done this?
Any tips or concerns would be appreciated
Thanks


This topic has 3 replies

CF

Chris Friesen

in reply to i82much on 08/02/2008 7:24 AM

08/02/2008 12:11 PM

i82much wrote:
> I am working on a project that is African Mahogany framed with
> Purpleheart.I was concerned if I needed to treat the edge that I'm
> going to glue, because of the oils (like Teak). It was suggested that
> I fume the purpleheart with muratic acid.

I edged some maple plywood with purpleheart for a storage-box lid a few
years ago using basic yellow wood glue. No special treatment for the
purpleheart.

So far it's held up just fine with more-or-less daily use.

Chris

rp

r payne

in reply to i82much on 08/02/2008 7:24 AM

09/02/2008 2:43 AM



i82much wrote:

> I am working on a project that is African Mahogany framed with
> Purpleheart.I was concerned if I needed to treat the edge that I'm
> going to glue, because of the oils (like Teak). It was suggested that
> I fume the purpleheart with muratic acid.
> I had seen the fuming process done with ammonia, but never with acid.
> Has anyone ever done this?
> Any tips or concerns would be appreciated
> Thanks

Fuming is generally done to fix or change the color. I've used
purpleheart a couple of times and had no problems with glueing. It did
not seem particularlly oily (like the cocobolo I used once), but wiping
with acetone or maybe alcohol should mitigate any oil problem that may
be.

ron

JC

"J. Clarke"

in reply to i82much on 08/02/2008 7:24 AM

08/02/2008 12:52 PM

i82much wrote:
> I am working on a project that is African Mahogany framed with
> Purpleheart.I was concerned if I needed to treat the edge that I'm
> going to glue, because of the oils (like Teak). It was suggested
> that
> I fume the purpleheart with muratic acid.
> I had seen the fuming process done with ammonia, but never with
> acid.
> Has anyone ever done this?
> Any tips or concerns would be appreciated

Bond it fresh cut (from the jointer, planer, or glueline rip blade,
not sanded) with a good epoxy and it should be fine. Sanding in
principle will heat the surface and bring up the oils. A solvent wipe
is said to do the same. So will letting it sit after cutting.

If Steven Knight tells you different, believe him--he's got more
experience with exotic woods than I do--but that's the advice I've
been following and so far it's working.

I've never heard of fuming being done to promote an adhesive bond.
HCl fuming is supposed to change the color of Purpleheard to
"cranberry" though. Something I may give a try sometime.


--
--
--John