I have read all archives regarding Tung Oil in this NG since January
this year from kind, helpful and experienced users.
I have another question, let say I need to finished FAST some small
walnuts and oaks part. This is what I planned to do: I will apply the
parts with Tung oil mixtures (50% Tung oil 50% paint thinner) and wipe
all excess oil. It should dry in an hour, sand lightly with #0000
steel wool. Apply first coats of Polyurethane, wait for 24 hrs sand it
again before applying another coat of polyurethane and so on until I
get the finishes I need.
My question, can I speed up the process if I apply a heat gun
(carefully) on the parts to increase the temperature? What would you
do to speed up the process rather than waiting 24 hrs according to
instruction from Woodcraft's 100% pure Tung oil? I may apply three
polyurethane coats or more that depend on the finished.
My garage temp for this time of the year is about 30 degrees to 50
degree and humidity below 50%. I could do leave the parts in the
house, temps from 68 to 70 degrees and humidity 1/2 setting. Your
advice most appreciated.
Thank you everyone
On Wednesday, December 8, 2004 at 10:58:59 PM UTC-5, G Yoder wrote:
> BlueDude wrote:
> > I have read all archives regarding Tung Oil in this NG since January
> > this year from kind, helpful and experienced users.
> >
> > I have another question, let say I need to finished FAST some small
> > walnuts and oaks part. This is what I planned to do: I will apply the
> > parts with Tung oil mixtures (50% Tung oil 50% paint thinner) and wipe
> > all excess oil. It should dry in an hour, sand lightly with #0000
> > steel wool. Apply first coats of Polyurethane, wait for 24 hrs sand it
> > again before applying another coat of polyurethane and so on until I
> > get the finishes I need.
> >
> > My question, can I speed up the process if I apply a heat gun
> > (carefully) on the parts to increase the temperature? What would you
> > do to speed up the process rather than waiting 24 hrs according to
> > instruction from Woodcraft's 100% pure Tung oil? I may apply three
> > polyurethane coats or more that depend on the finished.
> >
> > My garage temp for this time of the year is about 30 degrees to 50
> > degree and humidity below 50%. I could do leave the parts in the
> > house, temps from 68 to 70 degrees and humidity 1/2 setting. Your
> > advice most appreciated.
> >
> > Thank you everyone
> >
> >
> >
> Just a thought, you may just want to use WaterLox Original Sealer. Tung
> Oil base and provides a quick and very good finish. Check this link
> for further information.
> http://www.waterlox.com/product.cfm?productid=5
>
> George
Waterlox is an excellent product and well worth the $
You can also thin it with naptha and use japan drier as previously mentioned.
rick B.
There's an additive you can use called "Japan Drier." Adding a small
amount of these metalic salts will help your tung oil to cure faster.
A couple of tips - a little bit goes a long way. I'll use a capfull
added to a quart of finish (pure oil, oil and thinner mixed, or with or
without stain).
Don't mix more than you'll need, and don't re-mix any unused stuff with
your stockpile of finish.
One last thought ... you can also apply a spit coat of shellac over the
uncured tung oil. This will seal the oil (and smell) until it cures,
and makes a decent bond with any varnish (poly or otherwise) or top
coat.
Here's another alternative... if you're going to top coat with poly
anyway, then why not use a Sam Maloof finish and try a 50/50 mix of
tung oil and oil-based poly varnish? Apply it as you would the tung oil
... first coat thinned 50% with thinner ... just wipe it on (and wipe
the excess off). Repeat in 24 hours, and repeat THAT as necessary.
After about 3 to 5 coats, you'll start to building a finish. You can
then apply your poly straight until you build the finish you're looking
for.
best regards,
-Michael
On Sunday, May 20, 2018 at 7:34:33 PM UTC-4, Rick the antique guy wrote:
> On Monday, December 6, 2004 at 1:30:47 PM UTC-5, BlueDude wrote:
> > I have read all archives regarding Tung Oil in this NG since January
> > this year from kind, helpful and experienced users.
> >
> > I have another question, let say I need to finished FAST some small
> > walnuts and oaks part. This is what I planned to do: I will apply the
> > parts with Tung oil mixtures (50% Tung oil 50% paint thinner) and wipe
> > all excess oil. It should dry in an hour, sand lightly with #0000
> > steel wool. Apply first coats of Polyurethane, wait for 24 hrs sand it
> > again before applying another coat of polyurethane and so on until I
> > get the finishes I need.
> >
> > My question, can I speed up the process if I apply a heat gun
> > (carefully) on the parts to increase the temperature? What would you
> > do to speed up the process rather than waiting 24 hrs according to
> > instruction from Woodcraft's 100% pure Tung oil? I may apply three
> > polyurethane coats or more that depend on the finished.
> >
> > My garage temp for this time of the year is about 30 degrees to 50
> > degree and humidity below 50%. I could do leave the parts in the
> > house, temps from 68 to 70 degrees and humidity 1/2 setting. Your
> > advice most appreciated.
> >
> > Thank you everyone
>
> Yes blue Dude not under 60 deg F.whatever it takes.
> I assume You are NOT using water based Poly,
> which is not great over tung oil.
> Water based is not very compatible with Oils,
> even Oil solvent based stains.
> If You are NOT using a Spray Bomb of poly,
> thin Tung Oil and Poly or Varnish with naptha rather than Paint thinner,
> it evaps and dries faster.
> Also add Japan dryer available at most True value and Paint Stores to Tung Oil and Poly or Varnish, for fast curing times.
> If You are using solvent based Poly and Tung Oil about 1 teaspoon per Quart.
> *** Don't add it into the quart.
> That is just a proportion as in 1/8 teaspoon per 1/8 quart.
> ***Only mix what you are going to use on one application.
> Otherwise your Poly will gel and become unusable in 12 -24 hours.
> Heat lamps also work well but not too close keep at least 4 feet away well focused from above if possible. Keep a close watch sometimes it can create bubble. blisters.
> So only 1/2- 1 hour at a time with 15 minite breaks in between.
> The sun can also be Your friend on a dry day.
> Also give Your piece the same time and breaks as with the heat lamp.
> I am generally not in favor of blow dryers other than to crackle a finish.
> I hope this has been helpful.
>
> One last thing my dad taught me "Don't hurry unless You want to do it over".
> May the grain be with You
> rick B.
Rick,
I doubt Blue Dude is hurrying. His post is from 14 years ago. ;-)
If you're using oil-based poly, disregard the first step with the tung. The
oil in them will get help polymerizing from the resins and driers.
"BlueDude" <[email protected]> wrote in message
news:[email protected]...
>
> I have read all archives regarding Tung Oil in this NG since January
> this year from kind, helpful and experienced users.
>
> I have another question, let say I need to finished FAST some small
> walnuts and oaks part. This is what I planned to do: I will apply the
> parts with Tung oil mixtures (50% Tung oil 50% paint thinner) and wipe
> all excess oil. It should dry in an hour, sand lightly with #0000
> steel wool. Apply first coats of Polyurethane, wait for 24 hrs sand it
> again before applying another coat of polyurethane and so on until I
> get the finishes I need.
>
> My question, can I speed up the process if I apply a heat gun
> (carefully) on the parts to increase the temperature? What would you
> do to speed up the process rather than waiting 24 hrs according to
> instruction from Woodcraft's 100% pure Tung oil? I may apply three
> polyurethane coats or more that depend on the finished.
>
> My garage temp for this time of the year is about 30 degrees to 50
> degree and humidity below 50%. I could do leave the parts in the
> house, temps from 68 to 70 degrees and humidity 1/2 setting. Your
> advice most appreciated.
>
> Thank you everyone
>
>
>
On Monday, December 6, 2004 at 1:30:47 PM UTC-5, BlueDude wrote:
> I have read all archives regarding Tung Oil in this NG since January
> this year from kind, helpful and experienced users.
>
> I have another question, let say I need to finished FAST some small
> walnuts and oaks part. This is what I planned to do: I will apply the
> parts with Tung oil mixtures (50% Tung oil 50% paint thinner) and wipe
> all excess oil. It should dry in an hour, sand lightly with #0000
> steel wool. Apply first coats of Polyurethane, wait for 24 hrs sand it
> again before applying another coat of polyurethane and so on until I
> get the finishes I need.
>
> My question, can I speed up the process if I apply a heat gun
> (carefully) on the parts to increase the temperature? What would you
> do to speed up the process rather than waiting 24 hrs according to
> instruction from Woodcraft's 100% pure Tung oil? I may apply three
> polyurethane coats or more that depend on the finished.
>
> My garage temp for this time of the year is about 30 degrees to 50
> degree and humidity below 50%. I could do leave the parts in the
> house, temps from 68 to 70 degrees and humidity 1/2 setting. Your
> advice most appreciated.
>
> Thank you everyone
Yes blue Dude not under 60 deg F.whatever it takes.
I assume You are NOT using water based Poly,
which is not great over tung oil.
Water based is not very compatible with Oils,
even Oil solvent based stains.
If You are NOT using a Spray Bomb of poly,
thin Tung Oil and Poly or Varnish with naptha rather than Paint thinner,
it evaps and dries faster.
Also add Japan dryer available at most True value and Paint Stores to Tung Oil and Poly or Varnish, for fast curing times.
If You are using solvent based Poly and Tung Oil about 1 teaspoon per Quart.
*** Don't add it into the quart.
That is just a proportion as in 1/8 teaspoon per 1/8 quart.
***Only mix what you are going to use on one application.
Otherwise your Poly will gel and become unusable in 12 -24 hours.
Heat lamps also work well but not too close keep at least 4 feet away well focused from above if possible. Keep a close watch sometimes it can create bubble. blisters.
So only 1/2- 1 hour at a time with 15 minite breaks in between.
The sun can also be Your friend on a dry day.
Also give Your piece the same time and breaks as with the heat lamp.
I am generally not in favor of blow dryers other than to crackle a finish.
I hope this has been helpful.
One last thing my dad taught me "Don't hurry unless You want to do it over".
May the grain be with You
rick B.
On Monday, May 21, 2018 at 10:18:30 AM UTC-4, Leon wrote:
> On 5/21/2018 7:31 AM, Rick the antique guy wrote:
> > On Sunday, May 20, 2018 at 11:24:52 PM UTC-4, DerbyDad03 wrote:
> >> On Sunday, May 20, 2018 at 7:34:33 PM UTC-4, Rick the antique guy wrote:
> >>> On Monday, December 6, 2004 at 1:30:47 PM UTC-5, BlueDude wrote:
> >>>> I have read all archives regarding Tung Oil in this NG since January
> >>>> this year from kind, helpful and experienced users.
> >>>>
> >>>> I have another question, let say I need to finished FAST some small
> >>>> walnuts and oaks part. This is what I planned to do: I will apply the
> >>>> parts with Tung oil mixtures (50% Tung oil 50% paint thinner) and wipe
> >>>> all excess oil. It should dry in an hour, sand lightly with #0000
> >>>> steel wool. Apply first coats of Polyurethane, wait for 24 hrs sand it
> >>>> again before applying another coat of polyurethane and so on until I
> >>>> get the finishes I need.
> >>>>
> >>>> My question, can I speed up the process if I apply a heat gun
> >>>> (carefully) on the parts to increase the temperature? What would you
> >>>> do to speed up the process rather than waiting 24 hrs according to
> >>>> instruction from Woodcraft's 100% pure Tung oil? I may apply three
> >>>> polyurethane coats or more that depend on the finished.
> >>>>
> >>>> My garage temp for this time of the year is about 30 degrees to 50
> >>>> degree and humidity below 50%. I could do leave the parts in the
> >>>> house, temps from 68 to 70 degrees and humidity 1/2 setting. Your
> >>>> advice most appreciated.
> >>>>
> >>>> Thank you everyone
> >>>
> >>> Yes blue Dude not under 60 deg F.whatever it takes.
> >>> I assume You are NOT using water based Poly,
> >>> which is not great over tung oil.
> >>> Water based is not very compatible with Oils,
> >>> even Oil solvent based stains.
> >>> If You are NOT using a Spray Bomb of poly,
> >>> thin Tung Oil and Poly or Varnish with naptha rather than Paint thinner,
> >>> it evaps and dries faster.
> >>> Also add Japan dryer available at most True value and Paint Stores to Tung Oil and Poly or Varnish, for fast curing times.
> >>> If You are using solvent based Poly and Tung Oil about 1 teaspoon per Quart.
> >>> *** Don't add it into the quart.
> >>> That is just a proportion as in 1/8 teaspoon per 1/8 quart.
> >>> ***Only mix what you are going to use on one application.
> >>> Otherwise your Poly will gel and become unusable in 12 -24 hours.
> >>> Heat lamps also work well but not too close keep at least 4 feet away well focused from above if possible. Keep a close watch sometimes it can create bubble. blisters.
> >>> So only 1/2- 1 hour at a time with 15 minite breaks in between.
> >>> The sun can also be Your friend on a dry day.
> >>> Also give Your piece the same time and breaks as with the heat lamp.
> >>> I am generally not in favor of blow dryers other than to crackle a finish.
> >>> I hope this has been helpful.
> >>>
> >>> One last thing my dad taught me "Don't hurry unless You want to do it over".
> >>> May the grain be with You
> >>> rick B.
> >>
> >> Rick,
> >>
> >> I doubt Blue Dude is hurrying. His post is from 14 years ago. ;-)
> >
> > Hey I better learn how to navigate better and Check the dates Huh!
> > rick B
> >
> LOL, Unfortunately that information is not always obvious and if you are
> like me you may not want to go to the trouble to determine the age of
> the post every time.
Even though GG prominently shows the dates, I can typically spot an out-dated thread before
I even open it. When I see an unfamiliar Subject Line and notice that the thread contains
10, 20, sometimes 30 posts, that's usually a big hint. I check the wRec fairly often, so it's
rare that a thread gets to10, 20, (never) 30 posts before I've looked at it at least once.
I'm not sure if that works with other Usenet readers, but it's a clear sign of an old thread
when using GG.
On Sunday, May 20, 2018 at 11:24:52 PM UTC-4, DerbyDad03 wrote:
> On Sunday, May 20, 2018 at 7:34:33 PM UTC-4, Rick the antique guy wrote:
> > On Monday, December 6, 2004 at 1:30:47 PM UTC-5, BlueDude wrote:
> > > I have read all archives regarding Tung Oil in this NG since January
> > > this year from kind, helpful and experienced users.
> > >
> > > I have another question, let say I need to finished FAST some small
> > > walnuts and oaks part. This is what I planned to do: I will apply the
> > > parts with Tung oil mixtures (50% Tung oil 50% paint thinner) and wipe
> > > all excess oil. It should dry in an hour, sand lightly with #0000
> > > steel wool. Apply first coats of Polyurethane, wait for 24 hrs sand it
> > > again before applying another coat of polyurethane and so on until I
> > > get the finishes I need.
> > >
> > > My question, can I speed up the process if I apply a heat gun
> > > (carefully) on the parts to increase the temperature? What would you
> > > do to speed up the process rather than waiting 24 hrs according to
> > > instruction from Woodcraft's 100% pure Tung oil? I may apply three
> > > polyurethane coats or more that depend on the finished.
> > >
> > > My garage temp for this time of the year is about 30 degrees to 50
> > > degree and humidity below 50%. I could do leave the parts in the
> > > house, temps from 68 to 70 degrees and humidity 1/2 setting. Your
> > > advice most appreciated.
> > >
> > > Thank you everyone
> >
> > Yes blue Dude not under 60 deg F.whatever it takes.
> > I assume You are NOT using water based Poly,
> > which is not great over tung oil.
> > Water based is not very compatible with Oils,
> > even Oil solvent based stains.
> > If You are NOT using a Spray Bomb of poly,
> > thin Tung Oil and Poly or Varnish with naptha rather than Paint thinner,
> > it evaps and dries faster.
> > Also add Japan dryer available at most True value and Paint Stores to Tung Oil and Poly or Varnish, for fast curing times.
> > If You are using solvent based Poly and Tung Oil about 1 teaspoon per Quart.
> > *** Don't add it into the quart.
> > That is just a proportion as in 1/8 teaspoon per 1/8 quart.
> > ***Only mix what you are going to use on one application.
> > Otherwise your Poly will gel and become unusable in 12 -24 hours.
> > Heat lamps also work well but not too close keep at least 4 feet away well focused from above if possible. Keep a close watch sometimes it can create bubble. blisters.
> > So only 1/2- 1 hour at a time with 15 minite breaks in between.
> > The sun can also be Your friend on a dry day.
> > Also give Your piece the same time and breaks as with the heat lamp.
> > I am generally not in favor of blow dryers other than to crackle a finish.
> > I hope this has been helpful.
> >
> > One last thing my dad taught me "Don't hurry unless You want to do it over".
> > May the grain be with You
> > rick B.
>
> Rick,
>
> I doubt Blue Dude is hurrying. His post is from 14 years ago. ;-)
Hey I better learn how to navigate better and Check the dates Huh!
rick B
One thing that will work is to use a large cardboard box and cut a round
hole in it and stick a "hair dryer" in it and dry it this way. You would
have to check it to make sure it doesn't get too hot and burn anything....
Could use it in or out of the house. I have used this method and it works
pretty well.... just be careful and don't use a heat gun but use a cheap
hair dryer.
-Just an Idea.
"BlueDude" <[email protected]> wrote in message
news:[email protected]...
>
> I have read all archives regarding Tung Oil in this NG since January
> this year from kind, helpful and experienced users.
>
> I have another question, let say I need to finished FAST some small
> walnuts and oaks part. This is what I planned to do: I will apply the
> parts with Tung oil mixtures (50% Tung oil 50% paint thinner) and wipe
> all excess oil. It should dry in an hour, sand lightly with #0000
> steel wool. Apply first coats of Polyurethane, wait for 24 hrs sand it
> again before applying another coat of polyurethane and so on until I
> get the finishes I need.
>
> My question, can I speed up the process if I apply a heat gun
> (carefully) on the parts to increase the temperature? What would you
> do to speed up the process rather than waiting 24 hrs according to
> instruction from Woodcraft's 100% pure Tung oil? I may apply three
> polyurethane coats or more that depend on the finished.
>
> My garage temp for this time of the year is about 30 degrees to 50
> degree and humidity below 50%. I could do leave the parts in the
> house, temps from 68 to 70 degrees and humidity 1/2 setting. Your
> advice most appreciated.
>
> Thank you everyone
>
>
>
On Monday, May 21, 2018 at 11:04:16 AM UTC-4, DerbyDad03 wrote:
> On Monday, May 21, 2018 at 10:18:30 AM UTC-4, Leon wrote:
> > On 5/21/2018 7:31 AM, Rick the antique guy wrote:
> > > On Sunday, May 20, 2018 at 11:24:52 PM UTC-4, DerbyDad03 wrote:
> > >> On Sunday, May 20, 2018 at 7:34:33 PM UTC-4, Rick the antique guy wrote:
> > >>> On Monday, December 6, 2004 at 1:30:47 PM UTC-5, BlueDude wrote:
> > >>>> I have read all archives regarding Tung Oil in this NG since January
> > >>>> this year from kind, helpful and experienced users.
> > >>>>
> > >>>> I have another question, let say I need to finished FAST some small
> > >>>> walnuts and oaks part. This is what I planned to do: I will apply the
> > >>>> parts with Tung oil mixtures (50% Tung oil 50% paint thinner) and wipe
> > >>>> all excess oil. It should dry in an hour, sand lightly with #0000
> > >>>> steel wool. Apply first coats of Polyurethane, wait for 24 hrs sand it
> > >>>> again before applying another coat of polyurethane and so on until I
> > >>>> get the finishes I need.
> > >>>>
> > >>>> My question, can I speed up the process if I apply a heat gun
> > >>>> (carefully) on the parts to increase the temperature? What would you
> > >>>> do to speed up the process rather than waiting 24 hrs according to
> > >>>> instruction from Woodcraft's 100% pure Tung oil? I may apply three
> > >>>> polyurethane coats or more that depend on the finished.
> > >>>>
> > >>>> My garage temp for this time of the year is about 30 degrees to 50
> > >>>> degree and humidity below 50%. I could do leave the parts in the
> > >>>> house, temps from 68 to 70 degrees and humidity 1/2 setting. Your
> > >>>> advice most appreciated.
> > >>>>
> > >>>> Thank you everyone
> > >>>
> > >>> Yes blue Dude not under 60 deg F.whatever it takes.
> > >>> I assume You are NOT using water based Poly,
> > >>> which is not great over tung oil.
> > >>> Water based is not very compatible with Oils,
> > >>> even Oil solvent based stains.
> > >>> If You are NOT using a Spray Bomb of poly,
> > >>> thin Tung Oil and Poly or Varnish with naptha rather than Paint thinner,
> > >>> it evaps and dries faster.
> > >>> Also add Japan dryer available at most True value and Paint Stores to Tung Oil and Poly or Varnish, for fast curing times.
> > >>> If You are using solvent based Poly and Tung Oil about 1 teaspoon per Quart.
> > >>> *** Don't add it into the quart.
> > >>> That is just a proportion as in 1/8 teaspoon per 1/8 quart.
> > >>> ***Only mix what you are going to use on one application.
> > >>> Otherwise your Poly will gel and become unusable in 12 -24 hours.
> > >>> Heat lamps also work well but not too close keep at least 4 feet away well focused from above if possible. Keep a close watch sometimes it can create bubble. blisters.
> > >>> So only 1/2- 1 hour at a time with 15 minite breaks in between.
> > >>> The sun can also be Your friend on a dry day.
> > >>> Also give Your piece the same time and breaks as with the heat lamp.
> > >>> I am generally not in favor of blow dryers other than to crackle a finish.
> > >>> I hope this has been helpful.
> > >>>
> > >>> One last thing my dad taught me "Don't hurry unless You want to do it over".
> > >>> May the grain be with You
> > >>> rick B.
> > >>
> > >> Rick,
> > >>
> > >> I doubt Blue Dude is hurrying. His post is from 14 years ago. ;-)
> > >
> > > Hey I better learn how to navigate better and Check the dates Huh!
> > > rick B
> > >
> > LOL, Unfortunately that information is not always obvious and if you are
> > like me you may not want to go to the trouble to determine the age of
> > the post every time.
>
> Even though GG prominently shows the dates, I can typically spot an out-dated thread before
> I even open it. When I see an unfamiliar Subject Line and notice that the thread contains
> 10, 20, sometimes 30 posts, that's usually a big hint. I check the wRec fairly often, so it's
> rare that a thread gets to10, 20, (never) 30 posts before I've looked at it at least once.
>
> I'm not sure if that works with other Usenet readers, but it's a clear sign of an old thread
> when using GG.
This is all good information Folks.
I Joined this site : to learn from You and to share my learnigs.
Wood working Soup = planting /harvesting - to Nuts= the finished product. All parts are neccecary to the whole.
Much respect to You-all.
rick B.
"BlueDude" <[email protected]> wrote in message
> What would you
> do to speed up the process rather than waiting 24 hrs according to
> instruction from Woodcraft's 100% pure Tung oil?
Screw 'em. 23 hours is plenty.
>
> My garage temp for this time of the year is about 30 degrees to 50
> degree and humidity below 50%. I could do leave the parts in the
> house, temps from 68 to 70 degrees and humidity 1/2 setting. Your
> advice most appreciated.
Garage is way to cold for any oil finish that I'm aware of. This time of
year I brink my projects into the house and wait overnight to apply finish.
Ed
On 5/21/2018 7:31 AM, Rick the antique guy wrote:
> On Sunday, May 20, 2018 at 11:24:52 PM UTC-4, DerbyDad03 wrote:
>> On Sunday, May 20, 2018 at 7:34:33 PM UTC-4, Rick the antique guy wrote:
>>> On Monday, December 6, 2004 at 1:30:47 PM UTC-5, BlueDude wrote:
>>>> I have read all archives regarding Tung Oil in this NG since January
>>>> this year from kind, helpful and experienced users.
>>>>
>>>> I have another question, let say I need to finished FAST some small
>>>> walnuts and oaks part. This is what I planned to do: I will apply the
>>>> parts with Tung oil mixtures (50% Tung oil 50% paint thinner) and wipe
>>>> all excess oil. It should dry in an hour, sand lightly with #0000
>>>> steel wool. Apply first coats of Polyurethane, wait for 24 hrs sand it
>>>> again before applying another coat of polyurethane and so on until I
>>>> get the finishes I need.
>>>>
>>>> My question, can I speed up the process if I apply a heat gun
>>>> (carefully) on the parts to increase the temperature? What would you
>>>> do to speed up the process rather than waiting 24 hrs according to
>>>> instruction from Woodcraft's 100% pure Tung oil? I may apply three
>>>> polyurethane coats or more that depend on the finished.
>>>>
>>>> My garage temp for this time of the year is about 30 degrees to 50
>>>> degree and humidity below 50%. I could do leave the parts in the
>>>> house, temps from 68 to 70 degrees and humidity 1/2 setting. Your
>>>> advice most appreciated.
>>>>
>>>> Thank you everyone
>>>
>>> Yes blue Dude not under 60 deg F.whatever it takes.
>>> I assume You are NOT using water based Poly,
>>> which is not great over tung oil.
>>> Water based is not very compatible with Oils,
>>> even Oil solvent based stains.
>>> If You are NOT using a Spray Bomb of poly,
>>> thin Tung Oil and Poly or Varnish with naptha rather than Paint thinner,
>>> it evaps and dries faster.
>>> Also add Japan dryer available at most True value and Paint Stores to Tung Oil and Poly or Varnish, for fast curing times.
>>> If You are using solvent based Poly and Tung Oil about 1 teaspoon per Quart.
>>> *** Don't add it into the quart.
>>> That is just a proportion as in 1/8 teaspoon per 1/8 quart.
>>> ***Only mix what you are going to use on one application.
>>> Otherwise your Poly will gel and become unusable in 12 -24 hours.
>>> Heat lamps also work well but not too close keep at least 4 feet away well focused from above if possible. Keep a close watch sometimes it can create bubble. blisters.
>>> So only 1/2- 1 hour at a time with 15 minite breaks in between.
>>> The sun can also be Your friend on a dry day.
>>> Also give Your piece the same time and breaks as with the heat lamp.
>>> I am generally not in favor of blow dryers other than to crackle a finish.
>>> I hope this has been helpful.
>>>
>>> One last thing my dad taught me "Don't hurry unless You want to do it over".
>>> May the grain be with You
>>> rick B.
>>
>> Rick,
>>
>> I doubt Blue Dude is hurrying. His post is from 14 years ago. ;-)
>
> Hey I better learn how to navigate better and Check the dates Huh!
> rick B
>
LOL, Unfortunately that information is not always obvious and if you are
like me you may not want to go to the trouble to determine the age of
the post every time. Fortunately as you become more accustomed to the
regulars here you will learn to be a little more cautious before giving
a long answer. A short answer is OK, if that person is still around he
will respond and then you can feel confident that he or she is still
among the living and might appreciate a detailed answer. ;!)
On Wed, 08 Dec 2004 21:19:12 -0700, buck wrote:
> Could use it in or out of the house. I have used this method and it works
> pretty well.... just be careful and don't use a heat gun but use a cheap
> hair dryer.
> -
Don't try it with shellac, though. You get little hard bubbles all over
your finish. damhikt
--
"Keep your ass behind you"
vladimir a t mad {dot} scientist {dot} com
On Mon, 06 Dec 2004 18:30:47 GMT, [email protected] (BlueDude)
wrote:
>
>I have read all archives regarding Tung Oil in this NG since January
>this year from kind, helpful and experienced users.
>
>I have another question, let say I need to finished FAST some small
>walnuts and oaks part. This is what I planned to do: I will apply the
>parts with Tung oil mixtures (50% Tung oil 50% paint thinner) and wipe
>all excess oil. It should dry in an hour, sand lightly with #0000
>steel wool. Apply first coats of Polyurethane, wait for 24 hrs sand it
>again before applying another coat of polyurethane and so on until I
>get the finishes I need.
>
>My question, can I speed up the process if I apply a heat gun
>(carefully) on the parts to increase the temperature? What would you
>do to speed up the process rather than waiting 24 hrs according to
>instruction from Woodcraft's 100% pure Tung oil? I may apply three
>polyurethane coats or more that depend on the finished.
>
>My garage temp for this time of the year is about 30 degrees to 50
>degree and humidity below 50%. I could do leave the parts in the
>house, temps from 68 to 70 degrees and humidity 1/2 setting. Your
>advice most appreciated.
>
>Thank you everyone
Unless someone here has got a really good trick, I'd suggest just
using something else. Tung Oil takes forever and a day to dry, even
in warm weather. Try one of the "natural" stains, they dry really
quickly, and look almost as good, IMO.
Aut inveniam viam aut faciam
BlueDude wrote:
> I have read all archives regarding Tung Oil in this NG since January
> this year from kind, helpful and experienced users.
>
> I have another question, let say I need to finished FAST some small
> walnuts and oaks part. This is what I planned to do: I will apply the
> parts with Tung oil mixtures (50% Tung oil 50% paint thinner) and wipe
> all excess oil. It should dry in an hour, sand lightly with #0000
> steel wool. Apply first coats of Polyurethane, wait for 24 hrs sand it
> again before applying another coat of polyurethane and so on until I
> get the finishes I need.
>
> My question, can I speed up the process if I apply a heat gun
> (carefully) on the parts to increase the temperature? What would you
> do to speed up the process rather than waiting 24 hrs according to
> instruction from Woodcraft's 100% pure Tung oil? I may apply three
> polyurethane coats or more that depend on the finished.
>
> My garage temp for this time of the year is about 30 degrees to 50
> degree and humidity below 50%. I could do leave the parts in the
> house, temps from 68 to 70 degrees and humidity 1/2 setting. Your
> advice most appreciated.
>
> Thank you everyone
>
>
>
Just a thought, you may just want to use WaterLox Original Sealer. Tung
Oil base and provides a quick and very good finish. Check this link
for further information.
http://www.waterlox.com/product.cfm?productid=5